Thulium antimonide

Base Information Edit
  • Chemical Name:Thulium antimonide
  • CAS No.:12039-33-7
  • Molecular Formula:SbTm
  • Molecular Weight:290.684
  • Hs Code.:
  • European Community (EC) Number:234-890-9
  • Mol file:12039-33-7.mol
Thulium antimonide

Synonyms:Thulium antimonide;antimony;thulium(3+);EINECS 234-890-9;12039-33-7;Antimony, compound with thulium (1:1);Sb.Tm;Thulium antimonide (TmSb)

Suppliers and Price of Thulium antimonide
Supply Marketing:Edit
Business phase:
The product has achieved commercial mass production*data from LookChem market partment
Manufacturers and distributors:
  • Manufacture/Brand
  • Chemicals and raw materials
  • Packaging
  • price
Total 3 raw suppliers
Chemical Property of Thulium antimonide Edit
Chemical Property:
  • Boiling Point:°Cat760mmHg 
  • Flash Point:°C 
  • Density:g/cm3 
  • Hydrogen Bond Donor Count:0
  • Hydrogen Bond Acceptor Count:0
  • Rotatable Bond Count:0
  • Exact Mass:289.83803
  • Heavy Atom Count:2
  • Complexity:0
Purity/Quality:

99% *data from raw suppliers

Safty Information:
  • Pictogram(s):  
  • Hazard Codes: 
MSDS Files:

SDS file from LookChem

Useful:
  • Canonical SMILES:[Sb].[Tm+3]
Technology Process of Thulium antimonide

There total 6 articles about Thulium antimonide which guide to synthetic route it. The literature collected by LookChem mainly comes from the sharing of users and the free literature resources found by Internet computing technology. We keep the original model of the professional version of literature to make it easier and faster for users to retrieve and use. At the same time, we analyze and calculate the most feasible synthesis route with the highest yield for your reference as below:

synthetic route:
Guidance literature:
In neat (no solvent); prereaction of starting materials in evacuated Mo-glass ampoules at 500°C for 1 week, pelletizing , heating in a sealed Ta-tube (under vac.) at 1500°C;
DOI:10.1016/0925-8388(94)90774-9
Guidance literature:
In melt; (inert atm.); heating 5:3 mixt. of thulium and antimony at 900°C for 24 h, arc melting; powder XRD;
DOI:10.1021/ic802464u
upstream raw materials:

thulium

antimony

cobalt

iron